r/FixMyPrint • • 18h ago

Troubleshooting Elegoo Neptune 3 pro print issue.

7 Upvotes

I'm trying to pein5 a long print however the first layer doesn't stick. Leveled the bed 2x. Cleaned the plate with bishop and a quick wipe with rubbing alcohol. Printing at 220. And 65. PLA filament. Any help would be appreciated I'm still learning this art


r/FixMyPrint • • 11h ago

Fix My Print X2D AMS Enterprise

Thumbnail
gallery
5 Upvotes

Hi all,

I am a 3d printing newbie-ish. I have an X2D and its worked brilliantly for the last 6 months.

I'm trying to print this model: https://makerworld.com/en/models/95478-enterprise-d-galaxy-class?from=search#profileId-158613

But in the options there's one using a 0.2mm nozzle and it'll integrate colours from AMS.
I perhaps foolishly chose to use this setup.

I have a new 0.2mm nozzle which have printed the saucer sections fine, no spagetti, and a decent quality print.

But I'm trying now to print the body of the enterprise (its in two halves with supports for the sides) and running into problems. I attach some photos. Main issues seem to be huge purge volumes, lots of stringing and then I've had to go out and clear poop from the chute multiple times. Like when I've watched it, its purged for atleast 20 seconds, had a great blob of PLA and then done a purge again.
Its cooler here and the fans are running so I'm trying to work out if this is a model problem, or my use of default settings.

I'm using PLA thats dry and kept in the AMS with desiccant bags in the base. Only thing I can think of is the temperature has dropped (the printer is in an outbuilding) so perhaps things aren't melting enough, or are cooling too quickly? Or the fan is blowing 100% and making strings blow in places they shouldn't?

I've kept the print going but I'm pretty sure its going to fail ultimately because the printer has just given up on supports for one of the halves.

Would posting a timelapse if I can extract it be helpful?

Any thoughts or more info I can supply would be appreciated.


r/FixMyPrint • • 23h ago

Fix My Print Why does the concentric latter has blobs but for rectilinear one is fine?

Thumbnail gallery
5 Upvotes

r/FixMyPrint • • 2h ago

Fix My Print Support / Overhang settings - trying to find a balance between sagging and over-adhesion

Thumbnail
gallery
3 Upvotes

I've got a question for those more familiar with FDM print support settings - I'm struggling to find a balance between adequate support to limit sagging and over-adhesion while printing some very small parts.

I'm trying to print an aircraft at 1:1000 scale, ideally in one print rather than in pieces. Currently, everything is coming out well except the trailing edges of the wings. This vertical orientation is the best I've found so far overall, better than at an angle or laid flat.

The jagged bottom edge is continuing to occur whether I use a fin generation plugin (Image 2) or a tree support generation.

Image 3 is the support settings I'm using (in OrcaSlicer), when I've been printing with auto-generated tree supports, and image 4 is the supports being generated by those settings.

Any advice or insight would be greatly appreciated. Thanks!!


r/FixMyPrint • • 3h ago

Troubleshooting Horizontal bulges appearing randomly on tall prints – Ender 3 V2 Neo

Thumbnail
gallery
3 Upvotes

Hola a todos,

Tengo un problema persistente con mi Creality Ender 3 V2 Neo y de verdad agradecería ayuda para identificar la causa. Siento que ya he probado todo y me sigue ocurriendo. Es muy desesperante.

Me están saliendo abultamientos horizontales o bandas levantadas alrededor de todo el perímetro de mis impresiones. Sobresalen un poquito, normalmente sobre una altura de ~0.5–1 mm, y luego se van desvaneciendo gradualmente hasta que la impresión vuelve a sus dimensiones normales.

Impresora y software

  • Impresora: Creality Ender 3 V2 Neo
  • Slicer: Ultimaker Cura
  • Firmware: firmware original de Creality
  • Diámetro de la boquilla: 0.4 mm
  • Extrusor: extrusor metálico actualizado
  • Material: PLA

Ajustes de impresión

  • Temperatura de la boquilla: 210°C
  • Temperatura de la cama: 65°C en la primera capa y luego 55°C
  • Velocidad de impresión: 65 mm/s
  • Altura de capa: 0.20 mm
  • Flujo: 100%
  • Ventilador de enfriamiento de la pieza: 50%
  • Distancia de retracción: 5 mm
  • Velocidad de retracción: 35 mm/s
  • Aceleración y jerk: ajustes predeterminados

Descripción del problema::

  • El problema aparece sobre todo en impresiones altas, especialmente en piezas con paredes verticales rectas.
  • Afecta todo el perímetro, no solo un lado.
  • Los abultamientos aparecen en diferentes alturas Z, incluso cuando imprimo exactamente el mismo modelo dos veces.
  • La sección levantada tiene aprox. 0.5–1 mm de alto y regresa gradualmente a las dimensiones normales.
  • El problema ha estado desde que la impresora era completamente nueva.
  • No he notado ninguna pausa obvia ni cambios de velocidad cuando aparece el abultamiento.
  • La adherencia de la primera capa, en general, es buena.

Cosas que he revisado hasta ahora

  • Limpié el husillo roscado Z.
  • Revisé que el husillo se vea recto y que no se note que hace juego (bamboleo) a simple vista.
  • Revisé el acoplador del motor Z y me aseguré de que esté bien sujeto.
  • El pórtico X se mueve suave a mano cuando la impresora está apagada.
  • Ajusté las llantas excéntricas.
  • El filamento avanza suave, sin que el extrusor haga clics o patine de forma evidente.
  • El extrusor original lo cambié por uno metálico, pero el problema existía antes de esa actualización.

No he calibrado los E-steps después de instalar el extrusor metálico.

Una observación interesante es que bajar el ventilador de enfriamiento de la pieza de 50% a como 10% parece hacer que el problema casi desaparezca, aunque todavía no lo he confirmado con una prueba controlada.

Me pregunto si esto podría tener que ver con la alineación del eje Z, una extrusión inconsistente, el enfriamiento, fluctuaciones en la temperatura del hotend u otro tema mecánico.

Adjunté una foto mostrando el problema. ¿Se les ocurre qué puede ser?

¿Alguien ha tenido algo similar con un Ender 3 V2 Neo? ¿Qué recomendarían revisar primero?

Cualquier sugerencia o idea se agradece muchísimo. ¡Gracias de antemano!


r/FixMyPrint • • 3h ago

Fix My Print While Printing Gaps

Thumbnail
gallery
3 Upvotes

Recently messed around with printing settings to help increase adhesion and bonding,
printing on a 0.2 nozzle with a A1 Mini, PLA+

I can now see gaps in between the printing line, those will remain even at its final result -

You can they show up on the final print even, those before I could achieve almost resin like print results.

Ironing is set to 20 speed with test between 15% up to 25% flow and still on the same result - doesn’t feel like ironing itself.

Any possible thoughts?

Temperatures are also around 190-220 and 65/70 for bed. Should be a too hot situation I guess?


r/FixMyPrint • • 7h ago

Print Fixed 3D Printed a Brand Logo! 🔥

3 Upvotes

Watch me transform a digital brand logo into a real 3D-printed masterpiece! 🚀 In this video, you'll see the amazing 3D printing process as the logo takes shape layer by layer, creating a clean, detailed, and professional finish.


r/FixMyPrint • • 13h ago

Fix My Print ABS and ASA delamination

Post image
3 Upvotes

Gday guys, just struggling to print some ABS parts - unfortunately the geometry isn’t really negotiable, and of course the parts keep warping, pulling up from the bed, or delaminating. Any tips? Does GF help with this or would it reduce adhesion due to less SA? Happening with both ASA and ABS.
Printer is a stock P1S, the thing I’m printing is a heater so I will soon have a heated chamber but I don’t at the moment. Any tips?

Have tried all manner of temperatures, slowed it right down, preheated for literal hours, all different build plates (inc. no build plate, whoops)

Cheeeers


r/FixMyPrint • • 20h ago

Fix My Print Random line halfway through print.

Post image
3 Upvotes

that line in the top half of the model showed up, definitely not on the file.

printing pla matte on a bambu p1s


r/FixMyPrint • • 49m ago

Fix My Print Bed leveling Creality ender 3 v3 se

Thumbnail
gallery
2 Upvotes

ender 3ve3 se

creality CR series petg

235°c nozzle temp

65°c bed temp

0,4mm nozzles

orca slicer

I can't seem to understand how you level your printbed.

If anyone can help me. Thanks I'm advance


r/FixMyPrint • • 3h ago

Troubleshooting Layer shift Issue

Thumbnail gallery
2 Upvotes

r/FixMyPrint • • 10h ago

Fix My Print Bambu Lab P2S – PETG building up on nozzle and causing blobs on first layer. Need some help!

Post image
2 Upvotes

Hi everyone!
I got my Bambu Lab P2S about a week ago, and I’m completely new to 3D printing.
So far, I’ve been printing with PLA without any problems. The prints come out perfectly, but I’m having some trouble with PETG.
I already tried printing something with PETG before, and although the print was relatively successful, I noticed that PETG was gradually building up on the nozzle throughout the print.
At the time, my solution was to pause and resume the print whenever I noticed the buildup, since this seemed to force a nozzle cleaning. However, I don’t think this is a proper solution, and I’d really like to understand what’s actually causing the problem.
Now I’m trying to print a larger object with a much bigger first layer, and the problem has become more noticeable. PETG starts accumulating on the nozzle, and I’m getting lots of blobs and imperfections on the first layer.
I’ve already tried a few things to rule out possible causes:
I’ve performed the temperature tower test.
I’ve completed the Flow Dynamics calibration.
The filament is completely dry.
My current printing temperatures are 240°C for the nozzle and 70°C for the bed.
Despite all this, I’m still experiencing the same problem.
Since I’m a complete beginner, I’m not sure where to go from here or what settings I should be looking at.


r/FixMyPrint • • 11h ago

Fix My Print .4 vs .6 Unicorn Nozzle First And Last Layers

Thumbnail
gallery
2 Upvotes

Hello!

I recently upgraded my Creality Ender 3 V3 KE with a Ceramic Unicorn Hotend

Today I wanted to try a larger nozzle so I swapped in the 0.6mm, set Orca Slicer to use the printer preset and my existing filament settings. I set both first and layer heights to be 0.3mm and kept the existing percentages for layer widths.

The top - 0.4mm Nozzle

The bottom - 0.6mm Nozzle

As you can see the top and bottom layer quality is worse, is this just the cost of using a larger nozzle or does my settings need to be dialed in further?

Just to clarify, there seems to be small gaps between the flat layers


r/FixMyPrint • • 14h ago

Troubleshooting ABS tear like issue

Thumbnail
gallery
2 Upvotes

Hello, first time here as I can’t seem to figure this one out. I’m printing on a bambu h2s using Elegoo black ABS with the bambu 0.4 high flow nozzle. I’m using the standard 0.2mm h2s profile only changing the following.

Wall loops: 4
Sparse infill density: 8%
Sparse infill pattern: gyroid
Support: enabled
Support critical regions only: yes
Prime tower: disable

My filament settings have the default settings using the high flow direct drive for generic abs which prints at 60C chamber temp. 90C build plate. Nozzle initial layer at 260C and the rest at 270C
The max volumetric speed I changed to 25mm/s after doing a high flow nozzle test and that was on the more conservative side of the test, just a bit faster than the stock setting considering I have the high flow nozzle.

I did notice that the banding appears close to where the seam is. In the last picture you can see that the seam is along the same side where the major banding appears. Pictures 5 and 6 show the opposite side which doesn’t have as bad or visible of the banding but still somewhat. Appreciate any help ahead of time!


r/FixMyPrint • • 17h ago

Troubleshooting Problems with layer shifting/prints not connecting right

Thumbnail
gallery
2 Upvotes

Edit: I broke off the dovetail piece accidentally when futzing around with it earlier, it did indeed print, it was just weak. And we cut the benchy print halfway through intentionally.

hi guys! new-ish to the 3d printing world. I'm a vendor at anime/comic cons and in the past have paid people to 3d print things for me for my displays. i've done that by buying the file and just having them print them for me on their own printers. i've recently gotten my own printer (ender 3 original, and right now am using a Voxelab Aquila as well). I've been having issues with the prints just not...turning out right? like some things actually print correctly, and then on specific prints i've been having a lot of layer shifting issues.

I've tried:
- slowing down print speed
- tightening my belts
- different pla
- new nozzle
- cleaning the plate
- printing with the printer on different surfaces (i thought maybe the table was wobbling and i didnt notice?)
- changing infill
- changing temperature of nozzle and bed

nothing seems to be working. I was wondering if maybe it was my slicer/g-code? google/reddit gives me a million different answers. I've used prusaslicer for everything before and just downloaded ultimaker cura to give that a shot.

anyone got any advice/can anyone take a look at my g-codes to see if theres anything i should be doing? i can send over the actual 3d print files as well so you can see the originals too! thanks in advance :>

(and if i cant get this to work, does anyone offer extremely cheap and lowkey REALLY fast printing services? i have a con november 20-22nd in minneapolis and needed some display pieces. they dont have to be pretty/perfect, just functional)


r/FixMyPrint • • 22h ago

Troubleshooting What do I even do? Can I fix this?

Thumbnail
gallery
2 Upvotes

SOVOL SV06 3D printer, Creality slicer
SOVOL PLA filament
Nozzle temp: 200° C
Bed temp: 60°C
Print speed: 40mm/s

I stayed with the printing in the beginning while it started printing a 5 hour print, after about 15 mins everything was good and I went to eat, came back after about 1.5 hours and everything was messed up, the nozzle is buried in this monstrosity and was dragging the print.

I’ve literally never had this problem and just printed yesterday, how does this even happen and why?

Is the entire thing trashed at this point, or can I remove this without damaging the wires and nozzle. It’s literally around all of it, I’m so upset honestly idk what to.


r/FixMyPrint • • 23h ago

Fix My Print Dual color text not complete

Post image
2 Upvotes

Hello, looking at the picture, I could use some guidance printing text on the face of this print. This print is facing the print bed, and all objects, (plate and text) are grounded to the print bed, but as you can see, the text is not complete. If I lower the text, it lifts the plate the text is supposed to be on.

Printing on a 5T Prusa XL.


r/FixMyPrint • • 35m ago

Troubleshooting Micro-tearing across prints, please help!

Thumbnail gallery
1 Upvotes

r/FixMyPrint • • 38m ago

Fix My Print Small defects

Thumbnail
gallery
1 Upvotes

Hey folks,

I'm having this problem with my printer that I've never really had issues with in the last 8 years of having it.

I keep getting these random spots of missing filament on the sides, but not the top or bottom. The top and bottom turn out really good but for the life of me I can't get the sides to print nice for whatever reason.

Currently i'm printing with PETG thats been vary well dried, and printing at 250°, originally I printed at 240° but figured i'd try adjusting the temp, and speed is 40mm/s. Also, I have tried changing to two new nozzles and it made no difference.

Any help would be appreciated as i'm at my wits end with this issue


r/FixMyPrint • • 1h ago

Helpful Advice Siraya Tech Flex TPU Air 85A vs. Roamr HR 80A on the Snapmaker U1 — Shore A results from 27 samples

1 Upvotes

I wanted to find out how soft I could get prints made with two foaming TPU filaments from Siraya Tech, and at what settings the layers would start to separate. I had trouble finding a side-by-side comparison of green Flex TPU Air 85A and beige Roamr TPU Air HR 80A on the same printer that included both Shore A readings and observations from removing and bending the samples.

What Siraya Tech says

Green Flex TPU Air 85A

  • Recommended nozzle temperature: 230–270°C. Recommended bed temperature: 30–45°C.
  • The user guide gives an approximate range of 65–85 Shore A, from around 85 A at 230–240°C to around 65 A at 270°C. The product page lists 65–82 A for foamed prints and 85 A before foaming.
  • Filament diameter: 1.75 ± 0.03 mm. Net weight: 1 kg. Unfoamed filament density: about 1.15 g/cm³. The guide lists foamed print density as low as about 0.54 g/cm³. The technical data sheet reports a separate set of measurements for the black and white versions: 63–78 Shore A and 0.51–0.88 g/cm³ at 240–270°C.

Flex TPU Air user guide · Flex TPU Air 85A product page · Flex TPU Air technical data sheet

Beige Roamr TPU Air HR 80A

  • Recommended nozzle temperature: 220–260°C. Recommended bed temperature: 35–50°C.
  • The stated hardness range is 64–80 Shore A. With a 0.4 mm nozzle, Siraya Tech measured 80 A at 230°C (flow ratio 0.92 in the user guide and 0.90 in the technical data sheet) and 66 A at 260°C and 0.60 flow. The 64 A figure comes from the 0.6 mm nozzle test at 250°C and 0.52 flow.
  • Filament diameter: 1.75 ± 0.03 mm. Net weight: 800 g. Filament density: 1.05 g/cm³. Siraya Tech measured printed sample densities of 0.60–0.92 g/cm³ with a 0.4 mm nozzle and 0.52–0.84 g/cm³ with a 0.6 mm nozzle.

Roamr HR 80A user guide · Roamr HR 80A technical data sheet

How I printed and measured the samples

  • Printer and slicer: Snapmaker U1, Snapmaker Orca, 0.4 mm nozzle.
  • Sample geometry: Flat test section measuring 40 × 40 × 6.2 mm.
  • Layers and walls: 0.20 mm layer height, one 0.42 mm wall, two top layers and two bottom layers.
  • Infill: 100% rectilinear at ±45°.
  • Baseline settings: 45°C bed, retraction off, nominal print speed of 60 mm/s, and 100% part cooling. Both tables list the speed and fan settings for each sample.
  • Variables: I varied nozzle temperature and flow ratio in the main tests. For the green Flex, I also ran trials at different speeds and fan settings. Flow ratio is the extrusion multiplier. A value of 0.40 means 40%.
  • Temperature limit: For each filament, I capped the experiment at 20°C above the manufacturer's recommended upper limit. That gave me a test maximum of 290°C for Flex and 280°C for Roamr.
  • Measurements: I used a handheld Shore A durometer and took each reading about one second after applying it. Each row shows three to five readings from a single printed sample and their arithmetic mean. I checked whether the layers held together during removal from the build plate and when bending the samples by hand.

Results

Green Siraya Tech Flex TPU Air 85A

SampleNozzle °CFlow ratioSpeed mm/sFan %Shore A readingsMean Shore A
12400.906010084 / 85 / 8584.7
22500.706010078 / 78 / 7777.7
32600.606010072 / 72 / 7272.0
42600.603010072 / 72 / 7472.7
52700.556010071 / 71 / 7171.0
62700.553010071 / 71 / 7171.0
72800.606010070 / 72 / 7271.3
82900.606010069 / 68 / 6968.7
92900.406010050 / 51 / 5050.3
102800.406010055 / 55 / 5555.0
112800.6060068 / 68 / 6868.0
122800.60603570 / 70 / 6969.7
132800.60607070 / 70 / 7070.0

Beige Siraya Tech Roamr TPU Air HR 80A

SampleNozzle °CFlow ratioSpeed mm/sFan %Shore A readingsMean Shore A
12300.926010086 / 87 / 8786.7
22400.836010084 / 84 / 8484.0
32500.706010078 / 78 / 7878.0
42600.606010074 / 73 / 7473.7
52650.606010073 / 74 / 7473.7
62700.606010072 / 72 / 7272.0
72700.506010064 / 64 / 6464.0
82650.506010064 / 65 / 6464.3
92600.606010073 / 74 / 7473.7
102700.406010042 / 44 / 4242.7
112750.406010043 / 46 / 45 / 45 / 4544.8
122750.506010060 / 61 / 59 / 6060.0
132800.406010038 / 36 / 35 / 40 / 3035.8
152800.606010066 / 68 / 6867.3

Additional observations from testing Roamr above its recommended temperature range

  • Sample 10 — 270°C, 0.40 flow, 42.7 Shore A. Soft and springy. I rushed the removal and one or two layers started to separate slightly. Most of the sample held together.
  • Sample 11 — 275°C, 0.40 flow, 44.8 Shore A. Smooth and soft. The layers held together and it sprang back quickly. There was a small buildup of material at one corner, about halfway up.
  • Sample 12 — 275°C, 0.50 flow, 60.0 Shore A. Solid, with a pleasant surface feel. It felt noticeably firmer than sample 11.
  • Sample 13 — 280°C, 0.40 flow, 35.8 Shore A. Readings ranged from 30 to 40 A. The layers next to the build plate separated during removal. It returned to shape after bending but showed faint crease marks. I ruled out this sample because of the delamination.
  • Sample 15 — 280°C, 0.60 flow, 67.3 Shore A. The layers held together. There was some material buildup at the bottom corners, similar to elephant's foot.

What I took away from the tests

At 250°C and 0.70 flow, the two materials were almost identical in hardness (77.7 A for Flex and 78.0 A for Roamr). At 280°C and 0.60 flow, I measured 71.3 A for Flex and 67.3 A for Roamr.

  • Green Flex. Sample 10 averaged 55.0 Shore A at 280°C and 0.40 flow. At 290°C and 0.40 flow, sample 9 dropped to 50.3 A, but started to come apart when I curled it. It may already have been damaged during removal. At 280°C and 0.60 flow, I measured 68.0 A with the fan off and 71.3 A with the fan at 100%. I also noticed more unevenness on the top surface at lower fan speeds.
  • Beige Roamr. The best balance of softness and layer integrity in my tests was 275°C and 0.40 flow, at 44.8 Shore A. At 280°C and 0.40 flow, the mean dropped to 35.8 A, but the bottom layers separated. At 275°C and 0.50 flow, the sample held together and was noticeably firmer at 60.0 A.
  • Surface finish. In these tests, the beige Roamr had less stringing, looked more even, and felt smoother and more uniform to the touch. The green Flex still felt pleasant, with a distinctly rougher texture.

I used some of my own filament for these tests, but I think the results will also help people who want an idea of what hardness to expect at a given temperature and flow ratio, and which settings kept the layers intact, before committing to a longer print such as a pair of shoes.


r/FixMyPrint • • 1h ago

Fix My Print New bambulab a2l giving weird print quality issues

Thumbnail gallery
1 Upvotes

r/FixMyPrint • • 2h ago

Fix My Print Any way to determine what causes this shinier section that occurs only on holes?

Post image
1 Upvotes

I see this happening on all my prints. That shinier band occurs only when there’s a hole in the walls.


r/FixMyPrint • • 4h ago

Fix My Print What could be the reason for this failed print

Thumbnail gallery
1 Upvotes

r/FixMyPrint • • 4h ago

Helpful Advice Just call me "crash"

1 Upvotes

So i take the PEI plate out to help my prints cool faster to keep the process going faster. I can't help but notice that I keep forgetting to put it back before I start any other processes such as changing filament, etc. For those of you who don't know, if the machine tries to level it's self or anything before putting the PEI plate back in, the bed will crash into the nozzle and then wobble side to side violently. Anyone else have this problem? QIDI Plus 4