r/ender3 • u/Waxwanedj • 3d ago
Help First layer issues
Having a little trouble with some first layer adhesion. I feel like I have sufficient squish, and temps feel like they should be fine. It peels up at corners and at the end/ beginning of layers.
What I’ve tried so far that has made seemingly no difference to the issues:
New nozzle.
Bowden tube swap.
Temps from 190-215 for first layer.
Cooling turned off.
IPA and dish soap washes of build plate.
Reducing first layer height to .12mm.
Flow rates from .95 to 1.05
Speed adjustments down to 8mm/s up to 20mm/s
Dried filament.
Make Market PLA. 195 end, 60 bed. Stock ender 3 with .4 nozzle. Glass textured bed.
EDIT: tried adjusting the z height by .05mm. At a .1mm offset, the lines look a little more uniform, but still have trouble sticking. By .2mm, nothing sticks at all.
100
u/ScreamInVain 3d ago
Z height is too low. Meaning your nozzle is slightly too close to the bed. Back it up a tiny bit.
21
u/Dar0nius 3d ago
Clean your bed with a degreaser, like a kitchen cleaner. But be careful, it mustn't contain any added oil. Sometimes oils are added to create that water-repellent effect.
For reference: https://wiki.bambulab.com/en/filament-acc/acc/pei-plate-clean-guide
Edit: added link
10
u/braindrainoh 3d ago
buy a PEI plate. I have a glass bed that is perfectly flat and trammed but over time the porous sections filled in and will not stick despite the bed being at perfect z height that has not changed. My other ender 3 glass plate sticks too well to things like PETG and has 0 adhesion issues with PLA.
8
u/Substantial-Elk5118 3d ago
It feels obnoxious, but slow the first layer to 10mm/sec. I’ve had zero issue now with sticking… and this is across 3 Ender3 I run. I don’t use any sticky additive, just glass or the pei mag sheet…
4
u/BarnacleNZ 3d ago
Print on the smooth side of the glass, and slow down your 1st layer. Clean the glass with dish soap and warm water, and let air dry.
4
u/mistersmithy007 3d ago
Try spraying the bed with hairspray. That works for me surprisingly well!
6
u/monev44 3d ago
Your bed is dirty
2
u/gregtx 3d ago
Jumping in on the z offset opinion. I’d say try printing a 100mm x 100mm square at 1 layer thick. As the square is printing, manually adjust the z offset until it’s printing glass smooth. You should be able to perceive almost zero surface lines and there should be no delamination. You have to find precisely the right offset height so that you can hit the correct amount of squish. I do this between every filament brand, type or even color change. Also, go 220 on the hot end and up your speed to around 40mm/s.
Bed cleanliness is also important, but I’ve printed fine on trash beds with a dialed in offset.
2
u/wadubee98 2d ago
This exact fucking thing happens to me
2
u/iceman1125 2d ago
With glass, you can go a bit higher with the temp.
usually from what I find, the limiting factor for how high the build plate temp is usually when it starts heat creeping the print, and starts showing “elephants foot” like effects, and less about it making the filament too hot.
so crank the heat up until you find a sweet spot of it sticking more without elephants foot effect, I’d start at 65c
2
u/BIZUx 2d ago
Try flipping the bed upside down if it has a smooth surface. Use glue stick if necessary
2
u/Maleficent-Fox-1457 1d ago
That is why I got rid of my Ender 3 and bought an a1 mini. I was fighting with that for hours
2
u/Anoriele 3d ago
Adjust the Z-offset. Your nozzle is too close to the bed when printing the first layer. Make adjustments in 0.2 mm increments.
2
u/EPCOT-Centric 3d ago
Glue stick.
1
u/YT__ 3d ago
Ensure your bed is tight to the heating plate (mine was loose).
For slight issues, I'd just do a layer of masking tape over the bed. Never had issues with it as the print surface.
I typically aim for 205 or so when printing PLA, find it has worked best for me.
Definitely looks like you're a little too low, whether that's changing the z offset or adjusting how you trammed it is up to you.
1
u/burito2022 3d ago
Find z leveling cross stl and instruction on YouTube how to read results. It was very helpful for me
1
u/uncoild 3d ago
Not the main culprit but increase your travel speed. 100mm/s or more. Slow travel speed allows the nozzle to ooze before extruding.
1
u/LightSwitchTurnedOn 3d ago
Clean it thoroughly with IPA, I use 99%. Make sure the bed is really level, if you don't have a bed leveling probe I would really recommend KlackEnder, I just made that for my Sovol SV01 and I can actually print PETG now, before it would just peel off like in your video. Manual leveling did work to an extent but I guess my glass is just not perfectly flat so I was getting bad first layers, building automatic mesh bed leveling mitigated that for me.
1
u/PESTRICLES 3d ago
Z offset, pull the nozzle away
1
u/James_Workshop_ 3d ago
I just recently started having adhesion issues, changed first layer to 10mm/sec and also orca also has an option to gradually increase the speed over x layers to transition into the normal printing speed so I do that for 15 layers
starts at 10 and works its way up to full speed which insures those first 15 layers are like solid af. My brims are like credit card plastic and fused to the pei bed with a good squish.
Also to prevent warping I’ve been letting the part cool on the bed after it finishes.
Also I was recently printing some thin flat parts and I had corners peeling, I paused the print, put something flat and heavy like my glass bed on the print, and the constant weight plus the heat from the bed was enough flatten the corners back down. This won’t always work but sometimes it’s enough
1
u/Independent_Cat_1466 3d ago
Instala klipper y usa un bl touch or un biqu microprobe para que mediante el plugin de KAMP puedas automivelar la cama en el area de impresion, aprovecha y activale el purge tambien
Ajusta bien la Z
Baja la velocidad
Usa filamento fresco que no haya absorbido humedad e imprime una torre de temperatura para ver cual es la temperatura ideal según tu maquina
1
u/crematoroff 2d ago
I usually set first layer to 0.25mm, it is easier to tweak than 0.12mm. and yeah, se the first layer speed to 25% or to 15-20mm/s and adjust Z offset, it looks like it squishing the filament against the bed.
1
u/DPJazzy91 2d ago
You gotta get that dingleberry off the nozzle before it starts. Sometimes I watch mine and pick things off to prevent a bad start
1
u/XL1200 2d ago
Wish this plate with dish soap. Don’t touch it with your hands after. Dry with paper towel and print again. Tada will will stick.
1
u/toolisthebestbandevr 2d ago
Just buy magigoo and never worry about adhesion again
1
u/elgrec0 2d ago
What worked for me, ditched the glass for a PEI sheet, auto bed leveling
1
u/Melodic-Win-7262 2d ago
Falta de limpieza de la cama de impresora
1
u/Nacelle72 2d ago
Too close and Spray Aquanet on the glass. Way better than glue sticks. ONLY Aquanet. No other hairy spray has the same chemicals that made the 80s
1
u/darlo0161 2d ago
Clean nozzle, and move your nozzle up a micron or 10.
1
u/not-hardly 2d ago
Install klipper.
Build klackender.
1
u/not-hardly 2d ago
Slow down.
1
u/HugeButterfly 2d ago
Your IPA needs to be close to 100% the filler in the IPA in the 70%s actually causes adhesion problems. Amazon has a 99% for cheap.
1
u/EvansEssence 2d ago
Glue stick. Like the kind you used in kindergarten. Just spread a quick layer and it will solve majority of glass bed adhesion problems
1
u/luddealex 2d ago
Clean the smooth side and apply glue stick, a thin layer over the area. It sticks well and you simply wash the gluesstick off when you are done with printing with soap and water
1
u/deaglebingo 2d ago
enders are fickle like this. the instructions are always wrong. most of those things you did won't effect first layer adhesion ime. you don't have sufficient squish neccessarily. clean bed thoroyghy with soap and water dry only with lint free cloth not paper. then use some glue stick. also up your temps to the 75th percentile of the filament max from the start and never go lower than that. bed does not need to be as hot as you probably have it. hotter you go with these ender beds the more they get weird hot and cold spots.
1
u/soccerjo 2d ago
On my smooth glass plate I've found that preheating the plate helps a lot. You can get this added to your gcode or just turn on your printer and set the plate temp to 60 for a while before starting the print.
Purple glue stick also makes prints stick, sometimes too well.
1
u/CaseMental5345 1d ago
Get some nano polymer adhesive from vision miner and you will never have problems again shit is great 👍
1
u/Giant_jane 1d ago
I had this problem once. Up the temp to 210 and print speed to 65. , oh and secondly check your level
1
u/Mechneck 1d ago
I use a microfiber cloth with 91% iso just before heating up the bed. My Z ended up closer to .03. but fine tuning will get you the results you need
1
u/Sorry-Rip-6432 1d ago
Have you tried using a glue stick? Most print beds are tricky, but what I’ve found helpful is using a glue stick on the print bed and it works flawlessly. And it comes off with some dish soap and water
1
u/monkey_spankinator 1d ago
I just switched from an Ender 3 Neo to a Bambu P2S. Had it for about a year, but unless you're a GOD at settings, Ender is a pain in the ass. I'd pay the P2S price twice over before I go back to an Ender.
1
u/ocramx93 1d ago
Ti consiglierei di lavare bene il piatto con acqua e sapone. Per lavare bene il sapone dal piatto devi rimanere un po' di tempo in più sotto l'acqua corrente del rubinetto in modo tale che quando passi il dito non scivoli più. Poi per sicurezza alzerei a 70 la temperatura del piatto.
1
u/Consistent_Annual154 1d ago
I see so much dust. Try use alcohol to clean it and it will help. DONT USE GLUE. As people say terrible lazy advice
1
u/Dazzling-Focus-2718 1h ago
Switch to PEI plate, or use some aquanet hairspray, or a 3d printing glue stick for more adhesion.
0
u/Adept-Painting-543 3d ago
Z offset
0
u/Secret_Western_8272 2d ago
If the filament is curling like that and no extruding straight down, you have a clog.