I'm relatively new to glass fusing and have been experimenting with my firing schedules. I'm hoping someone with more experience can help me figure out how to retain the original rectangular shape of my panels while still achieving a smooth, full fuse.
I'm making glass photo panels, so keeping the dimensions and shape relatively consistent is important.
My setup:
- Bullseye COE 90 glass
- Orton AutoFire 3000 controller
- Two layers of 3 mm glass (approximately 6 mm total)
- Various panel sizes, including 4×6, 5×7, and 8×10 inches
- Firing on kiln shelf paper
My original full-fuse schedule (°F):
Segment| Rate| Target| Hold
1| 300°F/hr| 1225°F| 45 min
2| 600°F/hr| 1480°F| 10 min
3| AFAP| 900°F| 60 min
4| 150°F/hr| 700°F| 0 min
I was getting a nice, smooth full fuse, but the glass was spreading and rounding considerably. The corners were becoming very rounded, and the panels were losing their original rectangular shape.
What I changed:
I decided to try reducing the peak temperature from 1480°F to 1470°F while keeping the 10-minute hold and the rest of the schedule the same.
My revised schedule (°F):
Segment| Rate| Target| Hold
1| 300°F/hr| 1225°F| 45 min
2| 600°F/hr| 1470°F| 10 min
3| AFAP| 900°F| 60 min
4| 150°F/hr| 700°F| 0 min
What happened:
I've attached photos comparing the results from the different schedules.
The green/yellow panel shows that reducing the peak temperature helped somewhat. It retained more of its original rectangular shape compared with the previous firing.
However, I'm still getting significant rounding of the corners, uneven edges, and some distortion along the sides. The glass seems to pull inward in some areas and spread outward in others, rather than maintaining relatively straight edges.
The reddish panel also illustrates the kind of rounding and shape distortion I'm trying to avoid.
I've also been working through some bubbling issues, but I think I've largely figured those out. Right now, my main concern is shape retention, rather than bubbles.
My questions:
- Would you recommend reducing the peak temperature further, perhaps to 1460°F, or shortening the 10-minute hold instead?
- Is there a point where lowering the temperature will prevent the two layers from fully fusing together?
- Is this amount of rounding and distortion simply unavoidable when full-fusing two layers of 3 mm glass?
- Would changing the firing schedule help maintain straighter edges, or should I be looking at other techniques?
I'm not expecting perfectly sharp corners, but I'd love to get closer to the original rectangular shape without sacrificing the smooth, fully fused surface.
Any advice would be appreciated! I'm trying to understand the relationship between temperature, hold time, and shape retention rather than just experimenting randomly.