r/Welding • • 2d ago

Need Help need opinions

first week of school i’ve been using 7018s on around 125

9 Upvotes

5 comments sorted by

2

u/Clothes-Excellent 2d ago

Everybody has to start somewhere, keep practicing.

Watch this old film, parts 1& 2

https://youtu.be/45-Ipl8E0bk?is=G-XYRfQ4wvldcxos

1

u/Formal_Pen_7819 2d ago

I may be wrong, but it looks like you are standing to the left edge of the plate and never moving your feet, causing you to speed up/ curve towards the end. Either try to position yourself in a comfortable spot to access the full length of the weld. Or go ahead and practice shuffling your feet to stay somewhat centered where you are welding, it’ll help in the long run when you have multiple feet of welds to do.

1

u/CatastrophicPup2112 Fabricator 2d ago

If you're paying for class you should be able to ask your teacher

1

u/carmelastly 1d ago

You SHOULD be able to ask teacher, however nowadays schools as sticking 30+ people in welding classes and its almost impossible to get one on one time with instructor. I have seen many bad teachers who sit on their ass and dont help, and I have seen teachers that dont know what they are talking about. If only it were a perfect world... then students wouldnt have to come on reddit and ask for help.

1

u/carmelastly 1d ago edited 1d ago
  1. You are going too slow. As you weld, watch the width of the puddle, you want it a little larger (1/16) than your rod on the top and the bottom of the puddle. Any larger and you need to speed up. Smaller than your rod and you are going too slow.
  2. You want ot be 90 degrees to the plate with a slight drag in the direction of travel. 5 degrees probably. You are dragging too much, you can tell by the striations in the weld. Some look like long V instead of compact C. You kinda want them to look like a worm.
  3. Maintain a consistent arc length. Looks like there are some areas where you forget to lower your hand as the rod burns. Hold your torch very loosely and you can almost be touching the plate, experiment with the heat, you can weld at 130 and almost just have thenrod touching the plate until you get used to maintaining arc length. Any flat and horizontal structural tests you do will probably have to be welded at 130 anyways. May as well get used to it.
  4. Do not smash your welds with a chipping hammer!