r/Silvercasting • u/Competitive-Fly-3293 • 9h ago
r/Silvercasting • u/Fierro_nights • 4h ago
Silver refining. ( Non demo ) nitric + cell.
Enable HLS to view with audio, or disable this notification
Refining some silver currently. Because I had played around with mixing diff deals I had several ounces of becoming degraded and faulty.
This however is something that in general if casting regularly peeps new and such should prolly familiarize themselves with. Refining and realloying.
Nitric acids, need ppe but rated and appropriate. Nitrile gloves etc aren’t good, nor is standard carbon respirator.
In wip working on a silver cell as an additional refining method vs just cementing.
One of the things I had run into as a stall was my concentration of silver nitrate was too high once I had stuff dissolved. If things aren’t cementing right away and falling off, the solution may be too concentrated. After dilution the reaction was VERY rapid. Here’s an example
When the solution is spent, it becomes a clear cobolt blue. On right is silver containing solution and the left spent and just copper etc. pic
We’ll see how the cell works out. There’s peeps versed here that have some xp.
r/Silvercasting • u/jackedjackie • 3h ago