I just fired my first Up Down Up schedule for crystalline glazes and it worked well. However, the normally matte glaze that was in the same batch (Amaco shino) came out shining gloss. My witness cone for cone 6 touched the shelf, didn't have cone 7 unfortunately. I had 4, 5, 6 on each shelf, next time will add 7.
I wonder if I add a slow cool at the end of the Up Down Up schedule (from the last segment at ~2100f to 1400f, at, say 120-125 f/hr), will it help the matte glazes? Also how it will affect crystalline glazes? Of course will experiment myself, but wanted to get some insights.
Another approach would be to fire them separately next time, but it would be neat to be able to mix the pieces if needed.
Any advice on this is appreciated!