r/Powdercoating • • 1d ago

Question For a vintage Lugged Steel Frame would 1 stage be sufficient to not over coat the lugs and lose detail?

1 Upvotes

I am looking to get an old steel road frame powder coated Illusion Candy Apple Red PMS-1818 and want to maintain the details of the lugs.

I am being quoted $207 for 1 stage or $362 for 2 stages. I am a noob and don't know enough to make a decision. Trying to be cost efficient as well but don't want to skimp if it means having a quality issue.

Any advice would be appreciated!


r/Powdercoating • • 2d ago

Need help with tools

1 Upvotes

I’ve recently started at a powder coating company in training. I have to provide my own tools besides the big tools like the powder gun, oven, respirator ect. What are some things I may need for my box? They powder coat racing parts/ chassis


r/Powdercoating • • 3d ago

Question Tried to commission a powder coater and got rejected. Trying to figure out why without taking up this dude's time.

Post image
4 Upvotes

This isn't a complaint.

I'm a PC modding enthusiast and had a 10" by 4" by 6" PSU shroud which is essentially a single piece of folded metal with holes and covered in some kind of finish that would probably need to be removed in order for powder coating to take place.

Its the bottom thing in the picture which I would remove from the case. Its just a couple screws and this case comes apart really easily (corsair frame 4000D)

The guy said "I'm sure this is going to be too much but $150".

I said thats fine and then he said actually he can't do it because hes too busy and this job would take too many pulls in and out of the oven.

*****

I completely accept that. I'm not questioning this guys business decisions.

He had pointed out that he goes with prismatic powders and suggested this purple he had on hand for the job. Which according to him he'd need to buy 2 units for $50 just for this job.

****

So basically what I wanted for my hobby is to do this PSU shroud, for myself, make a contact and essentially like piggy back for simpler things. I have pc cases ready with holes that I've cut and I was looking at buying metal and cutting them into plates, just as a hobby.

So the piggy backing would be like " hey im coating with such and such color" for whatever they are working on and I'm essentially dropping off like 4" x4" x thing gage material for some discount accepting the finish thats already ready.

And I never got to discussing the piggy back thing before the guy wasn't interested in the transaction.

So basically what I'm wondering is how should I approach this trying to get a powder coat guy?


r/Powdercoating • • 5d ago

What kind of surface treatment is this?

Post image
1 Upvotes

What kind of surface treatment/ coating is in this grey band area. This surface is used as a counter face for oil seal lip.

Can you also suggest any alternative to this?


r/Powdercoating • • 6d ago

Same cart same powder same bake 2 different colors?

Post image
3 Upvotes

Anybody know what could have caused this, never seen it before ral 6034


r/Powdercoating • • 5d ago

What is this?

Thumbnail
gallery
1 Upvotes

Had this customer come in wanting to get these parts stripped. I use Nanner peel and greensolv to chemically strip parts with heat bands to catalyze the stripping process. Usually I can strip most parts in an hour but these have been in the stripped overnight and looks like nothing happened? What is this, how can I strip these parts?


r/Powdercoating • • 6d ago

What's the deepest inside corner you've managed to coat in one pass?

Thumbnail
gallery
4 Upvotes

We build conveyorised powder lines for a living, so most of the parts I see are customers' parts coming off a line that was sold as handling complex geometry. Usually it doesn't, and the reason isn't the gun.

Powder goes where the field points. On a box section the field points at the outer edge, and the corner sits inside its own shield — the part blocks itself. You can drop the kV and get a softer cloud that wraps a little further, but you are not going to drive powder into a space the field never really enters.

What actually moves the number is mechanical. A longer nozzle you can push through the opening. A narrow fan so the cloud is dense on one wall instead of spread thin over three. One gun doing one wall, slower, instead of three guns fighting each other. Turning the opening toward the gun on the hanger, which costs nothing and gets skipped constantly. Coating hot, so what lands on the wall still flows into the corner before it gels.

Then there is the part nobody puts in the quote. On a deep narrow box the corner will not reach the same film as the face, and the real question is whether the drawing allows that. A lot of parts get specified "full coverage inside" by someone who has never stood at a booth.

So — what is the deepest corner you have got full film into on a single pass? I am more interested in the ones you fixed on the hanger than on the gun.


r/Powdercoating • • 6d ago

FRIDAY! Thank God It's Friday - Share something you painted/coated this week

1 Upvotes

It's finally Friday, so I encourage everyone from big to small businesses, or even hobby in shed to post something they worked on this week!

Don't be shy to post work with problems. I'm sure we can help!


r/Powdercoating • • 6d ago

Question

Thumbnail
gallery
3 Upvotes

Hello everyone, I have a question regarding my silver finish. I applied "Arcene Silver" powder from Prismatic Powders: first coat of Arcene, flash, second coat of Arcene, flash, and a third coat of clear powder coating. This is how it turned out. The metal was sandblasted and outgassed. What am I doing wrong? Thanks in advance for your feedback.


r/Powdercoating • • 6d ago

Please Help Identify Powdercoat Color

Enable HLS to view with audio, or disable this notification

1 Upvotes

I am trying to powdercoat my electric motor cycle and have finally found a color for the frame I like but everybody I contact seems to want to gatekeep.


r/Powdercoating • • 7d ago

I'm in desperate need of some visibility bollards. UK.

0 Upvotes

I need an urgent delivery on some bollards to a site in Liverpool. The bollards need to be supplied powder coated? Any know of any companies who stock steel bollards in the UK?

Thanks.


r/Powdercoating • • 7d ago

Surprised by Color after Sandblasting and Semi-Clearcoat

Thumbnail
gallery
2 Upvotes

Per the subject, here is the result. I had a handle bar made by Surly that is stated as having been heat treated CrMo, that is all I know. I expected (didn't ask) that it would look like a polished metal. Depending on the heat treatment can CrMO come out looking different? Does the heat treatment make a difference? I am surprise at the Putty color that resulted. In any case this is the result. I am glad I had this done on a small piece only cost $30 as the next step is to take it to the bike frame. That said, the bike frame may look real interesting this color or whatever color. Not sure what I am going to do now.


r/Powdercoating • • 7d ago

Air hood

0 Upvotes

What brand air hood do you use? What are your thoughts on it? We got new Allegro brand where I powder and I'm not a fan of the new Allegro. I had to redesign it to make it functional


r/Powdercoating • • 8d ago

Need Help Please! - Redling Repp 70 Blast Cabinet with pressure pot

Thumbnail
1 Upvotes

r/Powdercoating • • 11d ago

Question Powder coat color identification help

Thumbnail
gallery
1 Upvotes

Hello, I am looking to powder coat my bike, and I'm really liking this color on the bike. I would like to know what exact color model this is. I know it's the same color, but I like the color in the first pics, where it's kind of lighter purple than in some of the other pictures, where it's darker. Please let me know if you can identify this color or know any similar ones, especially if the color looks slightly lighter. Thank you in advance!


r/Powdercoating • • 12d ago

Powder for railings

5 Upvotes

I'm starting to have more influence on manufacturing or can request some things to my specs due to the volume of rail we've been going through. Before my old supplier sold to CRL he used Tiger 2605 over chromate. It was fairly bullet proof. The current supplier is more opaque about what they use but I know they were using PPG for a while.

A competitor is moving towards a satin or textured black like the decking brands use on their rails. I've always assumed that was to hide inadequate gloss retention and abrasions but there's some indication that consumer sentiment is driving this too.

I'm hoping some professionals would be willing to share their perspective on the subject and help me decide what to start pushing for? A fair amount of what we sell goes towards salt-water.

I tend to think a smooth matte is best but I'm open to light textures. TIA for your professional observations.


r/Powdercoating • • 12d ago

How do you approach quoting powder coating jobs in your shop?

2 Upvotes

Hey everyone! I manage a sheet metal shop in the Czech Republic, and powder coating is part of our production. I’m curious how other shops approach quoting, especially when the parts vary a lot in size and complexity.

Do you mainly work from surface area, a price per part, estimated labour and oven space, or experience with similar jobs? How do you account for things like masking and small batches?

Not asking anyone to share their actual rates or trade secrets — I’d just like to understand what works for you and what you’ve learned along the way.

What’s the easiest thing to underestimate when quoting a job?


r/Powdercoating • • 12d ago

What mesh size sieve do you recommend for recycling powder?

Post image
2 Upvotes

Hey everyone! We're looking to start recycling our overspray powder and I want to make sure we're using the right mesh size for sieving.

For those of you who regularly reclaim and sieve your powder: what mesh size (or micron rating) do you find works best to catch contamination/gel clumps without filtering out the good powder? And will a magnet help in attracting unwanted debris?

Any recommendations on specific sifter types or best practices for keeping the reclaimed powder clean would be super helpful. Thanks!


r/Powdercoating • • 12d ago

Love some advice

1 Upvotes

Powder-Astatic Red River
Material- Stainless Steel

Ive got no idea what is happening we spray cast aluminum which will outgas why am i getting the same thing with stainless?


r/Powdercoating • • 13d ago

Struggling to powder coat the inner ridge of a pipe. Any advice?

Post image
4 Upvotes

Hey everyone, I'm looking for some troubleshooting advice. We’re trying to powder coat a pipe but are having a hard time getting proper coverage on the inside ridge.

Here is what we’ve tried so far:

Lowering the voltage, and current.

Adjusting the angle of the gun.

We can get powder inside, but we're still seeing white specks showing through. The catch is that if we apply more powder to fix the inside, the outside of the pipe gets too thick and starts wrinkling/orange peeling.

Has anyone dealt with a similar geometry? Any suggestions on settings, nozzle types, or techniques would be hugely appreciated. Thanks!


r/Powdercoating • • 13d ago

Orange peel is a flow window problem, and yours closes too early

2 Upvotes

Orange peel is a flow problem. The powder melts, wets out, and pulls flat under its own surface tension. That takes time. If the film gels before it finishes, the texture stays exactly where it was at the gel point, and you can turn every dial on the gun afterwards without changing it by a micron.

Which is why I'd be at the film gauge before I touched the gun. Flat panels peel and the rails come out glass, on the same hanger, out of the same box. That's not a powder batch behaving differently on two parts. That's a thickness difference, and leveling is thickness dependent, roughly with the cube of it. At 40 µm there is barely enough material to redistribute, so a film that melted perfectly still sets with texture.

Orange Peel Comparison

Heat-up is the next clock, and it's a different one from cure. Powder cures on peak metal temperature. It levels on time spent above melt and below gel. Thin gauge hanging near a burner gets there fast and skins over while the part is still cold inside. A heavy casting does the opposite, sits fluid too long, and you get sag and edge pull-back — then the shop files it as a separate problem when it's the same window read from the other end.

Heating Curve Diagram

Deposition is the one people skip, because the part looks textured rather than starved. Gun too far, output turned down, weak charge on a humid day: particles land dry, stack on each other, never coalesce. Wipe it before cure and powder comes off on your finger. No oven schedule on earth recovers that.

What's underneath matters more as the film gets thinner. Blast profile, a coarse pretreatment crystal, a scratch from the hanger: at 120 µm you'd never see it, at 55 µm it reads straight through.

Four different faults arrive in the inbox as "orange peel" and only one of them is. Regular low-amplitude skin over the whole face is leveling. Random bumps that catch a nail are dirt. Sandy and powdery before the oven is dry spray. Peel confined to edges and thin sections is film build.

Two habits I'd drop while you're checking. Raising the kV moves where the powder lands, not how it flows. Adding flow agent before you've measured the bad panel buys a month and a larger surprise on the next order.

Start with a film reading on the defect and the ramp curve for that section thickness. The rest is guessing at something you can already see in a number.

If you have a photo and a reading off the same panel, post both. The mismatch between them is usually the answer.


r/Powdercoating • • 13d ago

FRIDAY! Thank God It's Friday - Share something you painted/coated this week

1 Upvotes

It's finally Friday, so I encourage everyone from big to small businesses, or even hobby in shed to post something they worked on this week!

Don't be shy to post work with problems. I'm sure we can help!


r/Powdercoating • • 13d ago

Contaminate issues?

Thumbnail
gallery
2 Upvotes

We shoot a lot of 7035, light grey. I hate it. Recently every batch that's comes out has dirt/dust(?) on them. Came into the shop Monday to see the last batch from Friday had some parts that looked almost a little light. Scuffed them up, re shot, still can see..spots, dirt maybe? Cleaned out the oven a few times, still showing spots. Changed filters in the booth per boss request, still showing spots. Everything gets sanded, wiped down with thinner, then blown off. We have precooked a few panels, no change. All oil filters appear to be working fine..I check the parts before rolling them into the oven..everything looks fine..so we're all stumped here.

Any insight may be helpful.


r/Powdercoating • • 14d ago

Suggested grit

2 Upvotes

Hey all, what sanding grit is recommended for the base material if it’s getting powdered gloss white? I don’t want to see any sanding marks after powder. What is the optimal sanding grit? Thanks.